I had these parts made for a project I am working on and the manufacturer claims they are 'autoclave dry carbon', which should mean pre-preg, but to my untrained eye it looks like regular vacuum bagged wet infusion. There are tiny bubbles along the edges and the outer clear resin layer seems thicker than what I would expect a pre-preg.

Are there any carbon experts out there that can help me identify what process they used to make these parts?

       
Reply
Jason B
J
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 6
Those parts look good. With infusion the carbon is rarely straight as an arrow like your parts. That looks prepreg. Am I right?
Edited 5 Years Ago by Jason B
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Charles Woo - 6 Years Ago
oekmont - 6 Years Ago
Charles Woo - 6 Years Ago
oekmont - 6 Years Ago
Charles Woo - 6 Years Ago
oekmont - 6 Years Ago
Charles Woo - 6 Years Ago
JasonFL - 6 Years Ago
Charles Woo - 6 Years Ago
JasonFL - 6 Years Ago
Jason B - 5 Years Ago
Hanaldo - 5 Years Ago
Jason B - 5 Years Ago
MarkMK - 5 Years Ago
Hanaldo - 5 Years Ago
matthieutje65 - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search