Hi all,

Just a quick one.
I infused some small items recently, approx 300mm x 150mm with:
650g 2 twil (mould surface)
3 layers of 200 unidirectional
Then top layer of 450 2
I then added peel ply and infusion mesh.

The top surface just about wetted out, but the mould surface didn’t wet at all.

Is there a particular problem I’m having or is there perhaps a way to slow the resin flow to allow it to saturate all layers?

Many thanks,

Bill

Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
DorsetBill - 5/1/2019 8:03:32 PM
Fasta - 4/23/2019 5:39:51 AM
I think it is your uni materials too.

You can add a layer of a woven cloth in between the uni layers to help the resin pass through better. 

Does anyone have a suggestion for the material/weight of the material to use in between layers?

Anything woven or stiched  as long as it creates a new feed path through in-between the uni layers.





Edited 6 Years Ago by Fasta
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
DorsetBill - 6 Years Ago
SleepingAwake - 6 Years Ago
JasonFL - 6 Years Ago
DorsetBill - 6 Years Ago
JasonFL - 6 Years Ago
DorsetBill - 6 Years Ago
DorsetBill - 6 Years Ago
JasonFL - 6 Years Ago
Rich (Staff) - 6 Years Ago
SleepingAwake - 6 Years Ago
Hanaldo - 6 Years Ago
Fasta - 6 Years Ago
DorsetBill - 6 Years Ago
JasonFL - 6 Years Ago
DorsetBill - 6 Years Ago
JasonFL - 6 Years Ago
DorsetBill - 6 Years Ago
JasonFL - 6 Years Ago
DorsetBill - 6 Years Ago
Fasta - 6 Years Ago
DANNYHOCKIN - 6 Years Ago
DorsetBill - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search