I have seen a couple ways of people doing it and still a little confused what is the best method. I am make a couple small things but the contours are a little complicated. I normally was using a VER gelcoat and let that tack and then lay they first layer but I want to make these without the gel coat and clear coat afterwards. I've seen people spraying a mist of resin on them to get a tack so the first layer will stick or people using a spray tack like super 77. My question if I PVA the surface of the mold then use a tack spray will that show on the surface of the part??  and if it does will I be able to clean it off so I can clear coat it. This might have been asked a ton of times but I searched a little and couldn't find a direct answer.  Also I am infusing with a VER RTM resin if that helps any
Edited 6 Years Ago by mym3
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
If you are using PVA, then a spray tack isnt going to be much of a problem as long as you dont use too much of it. The key is to be very light-handed with it, dont even spray it AT your mould surface, spray it above your mold surface so that the mist settles down onto your mould. 

As long as you use it sparingly, then it should clean off quite easily and wont be noticeable after you have sanded and cleared your part.
mym3
m
Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)
Group: Forum Members
Posts: 10, Visits: 188
Hanaldo - 1/13/2019 1:12:53 AM
If you are using PVA, then a spray tack isnt going to be much of a problem as long as you dont use too much of it. The key is to be very light-handed with it, dont even spray it AT your mould surface, spray it above your mold surface so that the mist settles down onto your mould. 

As long as you use it sparingly, then it should clean off quite easily and wont be noticeable after you have sanded and cleared your part.

again this is my first time not using a gel coat so after I pop it make sure to do a rather light sanding right?  To make sure I'm not sanding into the carbon. What grit would you suggest? I got a 3 inch DA and a 5 inch DA with just about all grits to 5000.  Or do you suggest wets sanding by hand?  And thank you for your response.

Edited 6 Years Ago by mym3
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search