I want to fix legs to a resin table which needs fixing directly into the resin approx 25mm thick.
What’s the best way to do this? Don’t want to crack it. This project has cost a lot as I’ve used 10kg of glasscast 50.
Can it be tapped as well? Or maybe just drilled and fit a threaded bush to screw some bolts into.
Any advice greatly appreciated
Reply
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
and a picture ...