Will the glasscast 3 make the glasscast 50 really glossy?
I’ve done main pour and sanded down to 2000 grit. It’s quite cloudy although I’ve not polished it yet.
If I just brushed over the glasscast 3, would it all come back to being transparent again?
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Yes it would, but so would a polish.  You would need to add a decent thickness of around 1.5mm plus of GlassCast 3 to ensure it self levels perfectly flat.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
Thanks warren. So let’s say I really roughly sanded the resin to let’s say an 80 grit (the resin has a depth of 30mm) then apply 2mm of the glasscast it would be totally transparent?