By Bhamoggy - 11/4/2018 3:08:27 PM
Will the glasscast 3 make the glasscast 50 really glossy? I’ve done main pour and sanded down to 2000 grit. It’s quite cloudy although I’ve not polished it yet. If I just brushed over the glasscast 3, would it all come back to being transparent again?
|
By Warren (Staff) - 11/6/2018 4:59:28 PM
Yes as the new resin fills in any scratches and dinks in the previous layer.
|
|