Hey everyone,

I have been infusing parts using a two mould method to reproduce a curved piece with smooth surfaces on both sides. Unfortunately, during my infusion, once the epoxy reaches the vacuum line side and it starts spurting bubbles into the catch pot (see the middle-right circle), small bubbles started to climb back up the resin line, which is connected to the resin feed pot (see bottom circle). I can't seem to get it to stop. During my first infusion of this part it did not have any adverse effects, but it still concerns me that air is:

a) apparently not all the air is moving towards the flow of vacuum - ie. towards the vacuum pump
b) there shouldn't be bubbles in there regardless. The only bubbles I could think of are ones that get mixed in with the epoxy and do not have a chance to off-gas out of the mixture before they are sucked into the part. I realized that a degassing chamber would help fix this, so I am going to build one.



And yes I just realized that you can't read the print so ignore that part of the picture haha.

Anyways, if anyone else has experience this, or knows what it may be, that would be a big help. It is unfortunate that it is a closed mould, as I cannot see the details of where these bubbles are coming from. Any help would be greatly appreciated.

-Mike-
Reply
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hear is one more thing to consider. When you degass you are exposing the epoxy to full 29.9 HG and what happens? It boils and out gases.

Now if we infuse with full vac 29.9 it stands to reason that it will expose the resin to full vac again and what's going to happen? It is going to boil in our part. So closest to the vacuum source is where you have your pin holes because it is exposed to full vac but the feed line side is no longer exposed.

So I have been in a habit of infusing at 24 HG where I know there will be no out gasing in the part.

What do you guys think of that?

Fred
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
prairiecustomcomposites - 13 Years Ago
fgayford - 13 Years Ago
prairiecustomcomposites - 13 Years Ago
prairiecustomcomposites - 13 Years Ago
fgayford - 13 Years Ago
neilb - 13 Years Ago
prairiecustomcomposites - 13 Years Ago
fgayford - 13 Years Ago
prairiecustomcomposites - 13 Years Ago
             thanks for sharing that information!
matthieutje65 - 13 Years Ago
fgayford - 13 Years Ago
Kevin-Lee - 13 Years Ago
Warren - 13 Years Ago
NikCFC - 13 Years Ago
fgayford - 13 Years Ago
prairiecustomcomposites - 13 Years Ago
fgayford - 13 Years Ago
Warren - 13 Years Ago
Leon - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search