Dear easycomposites,

I intend to do this Project, i was planning to do it withlike the skateboard tutorial you have on YouTube… just with thinner wood.

Do you have any ideas on how much layers i would probably Need?I was wondering also how the Wood could bend in future?? It should stay in hisshape.

The Rhino object would be my mould. Thickness, i dont know, probably 5-7mm?
Thanks alot! Franzis

  


Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The layup depends what you are trying to achieve.  4mm of laminate should be nice and strong.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Franz Mussner
Franz Mussner
Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)
Group: Forum Members
Posts: 10, Visits: 28
Warren (Staff) - 9/10/2018 3:13:07 PM
The layup depends what you are trying to achieve.  4mm of laminate should be nice and strong.


Hey Warren. i finished the mold! as its just a onetime project, i mean i just need it once, i am thinking about laminating the whole thing and then destroying the mold.
i could follow your laminating instructions but it would take some time and in the end i just need one piece, so its kind of not worth, to make laminate molds of the mould for beeing able to produce the object.
what  do you think? i hope i didnt conufse you that much!
oh one more question: is it possible to sand laminated objects? i mean is it easy to sand with polyester hardened chopped strtand mats ?


Franz Mussner
Franz Mussner
Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)
Group: Forum Members
Posts: 10, Visits: 28
Franz Mussner - 11/7/2018 1:05:42 PM
Warren (Staff) - 9/10/2018 3:13:07 PM
The layup depends what you are trying to achieve.  4mm of laminate should be nice and strong.


Hey Warren. i finished the mold! as its just a onetime project, i mean i just need it once, i am thinking about laminating the whole thing and then destroying the mold.
i could follow your laminating instructions but it would take some time and in the end i just need one piece, so its kind of not worth, to make laminate molds of the mould for beeing able to produce the object.
what  do you think? i hope i didnt conufse you that much!
oh one more question: is it possible to sand laminated objects? i mean is it easy to sand with polyester hardened chopped strtand mats ?



as the mould is a spiral , i probably need to destroy it to release it from the laminate because it will lock with the laminate