Dear easycomposites,

I intend to do this Project, i was planning to do it withlike the skateboard tutorial you have on YouTube… just with thinner wood.

Do you have any ideas on how much layers i would probably Need?I was wondering also how the Wood could bend in future?? It should stay in hisshape.

The Rhino object would be my mould. Thickness, i dont know, probably 5-7mm?
Thanks alot! Franzis

  


Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Looks like it could be a nightmare!

If you can CNC a core , then you can use that to make a mould and then work from there.

Making the wooden core would be a case of using thin strips of wood bonded together -  using the mould as a template.  The strips would need to be thin enough to easily curve around.  You would clamp it top and bottom and in various places then build up the strips of wood to get the shaped core in wood.

Once youve done that, the infusion would be simple by comparison!


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Franz Mussner
Franz Mussner
Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)
Group: Forum Members
Posts: 10, Visits: 28
Warren (Staff) - 9/10/2018 12:19:43 PM
Looks like it could be a nightmare!

If you can CNC a core , then you can use that to make a mould and then work from there.

Making the wooden core would be a case of using thin strips of wood bonded together -  using the mould as a template.  The strips would need to be thin enough to easily curve around.  You would clamp it top and bottom and in various places then build up the strips of wood to get the shaped core in wood.

Once youve done that, the infusion would be simple by comparison!

thanks Warren for the fast answer!
the mould i was thinking to do it in that style with 3mm deep carton and styropor? as you guys show in this video  https://youtu.be/XeeSsmsm9h0
could work?
Franz Mussner
Franz Mussner
Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)
Group: Forum Members
Posts: 10, Visits: 28
Franz Mussner - 9/10/2018 2:04:27 PM
Warren (Staff) - 9/10/2018 12:19:43 PM
Looks like it could be a nightmare!

If you can CNC a core , then you can use that to make a mould and then work from there.

Making the wooden core would be a case of using thin strips of wood bonded together -  using the mould as a template.  The strips would need to be thin enough to easily curve around.  You would clamp it top and bottom and in various places then build up the strips of wood to get the shaped core in wood.

Once youve done that, the infusion would be simple by comparison!

thanks Warren for the fast answer!
the mould i was thinking to do it in that style with 3mm deep carton and styropor? as you guys show in this video  https://youtu.be/XeeSsmsm9h0
could work?

do you think i could do the object also without inner wood core and just go with fiber and flax?