Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Sheet
»
How flexible is the 0.25mm carbon sheet?
How flexible is the 0.25mm carbon sheet?
Post Reply
Like
11
How flexible is the 0.25mm carbon sheet?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Ledon Racing
Ledon Racing
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 12,
Visits: 74
Hello,
I'm hoping to be able to use the 0.25mm pre-preg sheet to wrap around 2" diameter tube, is it flexible enough to do that? It will then be bonded in place with epoxy resin.
Also are you still able to achieve a pin hole free surface finish on such a thin sheet?
I've seen that you do offer a 'flexible' sheet, but its only in plain weave and I'd much rather have it in a 2 x 2 twill.
Thanks,
Nathan
www.
LedonRacing
.com
Professional motorsport services
& composite production / repairs.
Reply
Like
11
Matt (Staff)
Matt (Staff)
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Hi Nathan,
Yes, you would be able to get the 0.25mm
pre-preg carbon fibre sheet
to wrap around a 2" diameter tube. It would of course have a prepensity to 'spring off' but providing it was keyed properly before bonding and then bonded well onto the tube then I don't think this would be a problem at all.
Also are you still able to achieve a pin hole free surface finish on such a thin sheet?
Yes, absolutely! The 0.25mm sheet has a perfect, pin-hole free surface just like the other thicknesses of pre-preg carbon fibre sheet we make.
I've seen that you do offer a 'flexible' sheet, but its only in plain weave and I'd much rather have it in a 2 x 2 twill.
We use plain weave because it's a 'flatter' weave than a 2/2 twill. We have made the flexible using twill in the past but the texture of the fabric tends to print-through quite a bit onto the surface of the flexible material meaning that the flatter the material inside, the flatter snd less textured the surface will be. For this reason, we don't press any 2/2 twill flexible anymore (well, not in the regular
thin flexible carbon fibre sheet
, but we do use a twill for our
thick flexible carbon fibre sheet
).
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Tags
carbon fibre
flexible
pre-preg
sheet
surface
Reply
Like
10
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
It's been 2 years!
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
11
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search