Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Sheet
»
How flexible is the 0.25mm carbon sheet?
How flexible is the 0.25mm carbon sheet?
Post Reply
Like
11
How flexible is the 0.25mm carbon sheet?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Ledon Racing
Ledon Racing
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 12,
Visits: 74
Hello,
I'm hoping to be able to use the 0.25mm pre-preg sheet to wrap around 2" diameter tube, is it flexible enough to do that? It will then be bonded in place with epoxy resin.
Also are you still able to achieve a pin hole free surface finish on such a thin sheet?
I've seen that you do offer a 'flexible' sheet, but its only in plain weave and I'd much rather have it in a 2 x 2 twill.
Thanks,
Nathan
www.
LedonRacing
.com
Professional motorsport services
& composite production / repairs.
Reply
Like
11
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How flexible is the 0.25mm carbon sheet?
Ledon Racing
-
14 Years Ago
Hi Nathan, Yes, you would be able to get the 0.25mm pre-preg carbon fibre sheet to wrap around a...
Matt (Staff)
-
14 Years Ago
It's been 2 years!
ajb100
-
12 Years Ago
Post Reply
Like
11
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search