By Ledon Racing - 9/27/2012 8:06:41 AM
Hello,
I'm hoping to be able to use the 0.25mm pre-preg sheet to wrap around 2" diameter tube, is it flexible enough to do that? It will then be bonded in place with epoxy resin.
Also are you still able to achieve a pin hole free surface finish on such a thin sheet?
I've seen that you do offer a 'flexible' sheet, but its only in plain weave and I'd much rather have it in a 2 x 2 twill.
Thanks,
Nathan
|
By ajb100 - 6/8/2014 12:03:39 AM
It's been 2 years!
|
|