Hi,
I'm a newbee in carbonfiber, I want to do some parts by it and I have a cnc machine to create the mould.

The cheapest material in access for me is wood, but I'm not sure if it is at all possible to use wood as mould material. Once I asked this from a carbonfiber seller on ebay and the answer was a big "No"!

I thought to write here may be somone may point me to a tutorial to turn wood to a mould or to teach me a material very cheap to use for mould and that I can put it under cnc.

My cnc machine can handle x=55cm, y=40cm, z=6cm, but untill now I only made things by wood and sometimes small aluminium shaft for hobby robots. I don't have access to aluminum for mould making.

Also sorry for my English, not native, may have mistakes.

Thank you.
Replies
Ledon Racing
Ledon Racing
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 12, Visits: 74
Why do you not have access to aluminium?

If you plan on making multiple parts, ally would be my material of choice every time, its easy to machine, you get a great surface finish and you don't have to ever worry about the mould breaking up.

www.LedonRacing.com

Professional motorsport services
& composite production / repairs.



Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Aluminium is quit expensive if you want to make a mould you need quit a big massive block of Aluminium Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Ledon Racing
Ledon Racing
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 12, Visits: 74
matthieutje65 (12/09/2012)
Aluminium is quit expensive if you want to make a mould you need quit a big massive block of Aluminium Smile


Yeah but his mill is only small, so I don't think he's going to be machining massive slabs of anything Smile

Ally compared to good quality PU or epoxy model board isn't actually too expensive, especially when you take into account the time it would take to get a compareable surface finish by sealing lesser quality materials. Also if you have a part that is dimensionally critical you don't really want to start adding resin / sealer to it in uncontrollable quantities.

www.LedonRacing.com

Professional motorsport services
& composite production / repairs.



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search