In simple moulding terms, you would be looking at a 2 part mould, split down the center-line into left and right moulds. The hard and fiddly bit is going to be getting the pre-preg into the mould properly and into the detail.
In terms of the actual design, it would almost certainly be worth doing some structural analysis on your design to determine any changes and also to test any ideas on layup to get a working design.