By Tyler Carr - 6/1/2018 10:31:31 PM
I am a professional inline speed skater and for my senior project want to work with carbon fiber to create my own frame.
I know how to use solid works and have a design idea, but I was wondering if anyone can help or give general advice on how to make a part like this from Prepreg carbon .
Thanks!!
|
By Warren (Staff) - 6/5/2018 4:07:39 PM
In simple terms yes, once you get around the fiddly aspect of it.
|
|