Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Complex mould piece (advice needed)
Complex mould piece (advice needed)
Post Reply
Like
3
Complex mould piece (advice needed)
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
JVP
J
JVP
posted 7 Years Ago
ANSWER
HOT
Topic Details
J
Group: Forum Members
Posts: 2,
Visits: 168
Hi! I just wanted some advice on how to go about making a mould of the part pictured below (circled red). I was considering using the uni-mould kit and obviously closing the hole but would this be the sufficient way to go about it? My plan is to replicate this part via a mould then make replicas of it with carbon fibre via resin infusion (not prepreg). Please advise if this is possible. Many thanks in advance.
Attachments
5663381802_10b128ea56_b.jpg
(
380 views,
299.00 KB
)
Reply
Like
3
Reply
Hanaldo
Hanaldo
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
It wouldn't be easy, but it's certainly possible. To be honest, the trickiest thing I see there will be the clips. Fairly straight forward otherwise, just a little tight.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Complex mould piece (advice needed)
JVP
-
7 Years Ago
It wouldn't be easy, but it's certainly possible. To be honest, the trickiest thing I see there will be the clips. Fairly straight forward otherwise, just a little tight.
Hanaldo
-
7 Years Ago
Thanks for the reply Hanaldo. Just out of curiosity, what do you think would be the best method? My only issue is that I'd create the mould using uni-mould but the mould would not have any...
JVP
-
7 Years Ago
Ifyou're concerned regarding some of the tight angular areas, then you could possibly try using an epoxy gelcoat and a combination of powder bound csm (with epoxy resin) and EC's mould making putty,....
MarkMK
-
7 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search