EM160, EMP160 Mould questions


Author
Message
ECV3
ECV3
Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)
Group: Forum Members
Posts: 30, Visits: 106
Can PVA be used as a release agent on the pattern for the initial cure then washed of the mould when the pattern is removed for the post cure ?.

What temperature will the mould reach in the initial cure ?.

How long is the shelf life ?.

Cheers.
Edited 9 Years Ago by ECV3
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The actual exotherm depends on a variety of factors. However in our experience, it has been fine on various foam based patterns which have a low HDT so I suspect you wouldn't have a problem with it reaching 65C. The Shelf life is 12 months from manufacture.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant