By ECV3 - 12/13/2017 2:46:44 PM
Can PVA be used as a release agent on the pattern for the initial cure then washed of the mould when the pattern is removed for the post cure ?.
What temperature will the mould reach in the initial cure ?.
How long is the shelf life ?.
Cheers.
|
By ECV3 - 12/14/2017 8:26:35 PM
Cheers Warren.
|
|