EM160, EMP160 Mould questions


Author
Message
ECV3
ECV3
Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)
Group: Forum Members
Posts: 30, Visits: 106
Can PVA be used as a release agent on the pattern for the initial cure then washed of the mould when the pattern is removed for the post cure ?.

What temperature will the mould reach in the initial cure ?.

How long is the shelf life ?.

Cheers.
Edited 9 Years Ago by ECV3
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Although PVA could be used for the room temperature cure, we would generally avoid it for high quality parts as PVA leaves slight surface marring which needs to be polished out.  A modern chemical release agent would be a better choice,


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ECV3
ECV3
Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)
Group: Forum Members
Posts: 30, Visits: 106
Warren (Staff) - 12/13/2017 5:34:46 PM
Although PVA could be used for the room temperature cure, we would generally avoid it for high quality parts as PVA leaves slight surface marring which needs to be polished out.  A modern chemical release agent would be a better choice,

Thanks,

Any idea what kind of temps the intial cure will reach as i'd like to mould a PLA plastic object that has a of tg 65ish ?. And the shelf life ?.
Cheers.