Hello,

Now, I am using Durepox Clear coat, and I need 3 layers at least to have good results.
I would like to decrease the number of layers, and I would like to know your experiences with different clearcoats.
Does someone know a high hiding clearcoat?

Vinz

Vinz
Reply
Jaspen
Jaspen
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 9, Visits: 24
oekmont - 10/20/2017 10:17:58 AM
If I want a real deep finish, I use basco lacquer. They also got clear filler, wich works brilliantly. But I am certainly no painting expert. Usually I'll leave this to a painter.

Hello

 I use MIPA CC9 High Solid Clear Coat. 2 layers prefect surface!