Hello,

Now, I am using Durepox Clear coat, and I need 3 layers at least to have good results.
I would like to decrease the number of layers, and I would like to know your experiences with different clearcoats.
Does someone know a high hiding clearcoat?

Vinz

Vinz
Reply
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Saff - 10/19/2017 9:50:56 AM
Vinz - 10/19/2017 5:44:29 AM
Hello,

Now, I am using Durepox Clear coat, and I need 3 layers at least to have good results.
I would like to decrease the number of layers, and I would like to know your experiences with different clearcoats.
Does someone know a high hiding clearcoat?

Vinz


for little parts I use 2k clear coat in rattle can, usually 1 or 2 layers gives me good result (depending on the quality surface). For bigger parts I ask to a professional car painter that use high solid high gloss clear coat.