+x oekmont - 10/20/2017 10:17:58 AMIf I want a real deep finish, I use basco lacquer. They also got clear filler, wich works brilliantly. But I am certainly no painting expert. Usually I'll leave this to a painter.
+x Saff - 10/19/2017 9:50:56 AM+x Vinz - 10/19/2017 5:44:29 AMHello,Now, I am using Durepox Clear coat, and I need 3 layers at least to have good results.I would like to decrease the number of layers, and I would like to know your experiences with different clearcoats.Does someone know a high hiding clearcoat?Vinzfor little parts I use 2k clear coat in rattle can, usually 1 or 2 layers gives me good result (depending on the quality surface). For bigger parts I ask to a professional car painter that use high solid high gloss clear coat.
+x Vinz - 10/19/2017 5:44:29 AMHello,Now, I am using Durepox Clear coat, and I need 3 layers at least to have good results.I would like to decrease the number of layers, and I would like to know your experiences with different clearcoats.Does someone know a high hiding clearcoat?Vinz