BMW HP4 RACE bike frame is made with ----- Resin Infusion! :-D


Author
Message
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Just to throw in a nice little tidbit of inside info in this forum -- touching on the endless discussion on how Resin infusion can compare to PRE-preg or other "Aerospace" methods

The process that BMW calls "Resin Transfer" and use for building 750 frames for the ultra high end - carbonfibre overload "HP4 RACE" version of the S1000RR bike  -- is an advanced resin infusion process -- using CNC machined moulds, and rather than "sucking in" the resin it is High pressure injected, like when doing plastic parts.

BMW says that this process is used to be able to control fibre orientation down to individual tow strands, in order to control torsional flex and optimize strength to weight ratio.

The outer layers are actually Biaxial CF cloth -- Smooooth

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 8 Years Ago by Dravis
Reply
FLD
FLD
FLD
posted 8 Years Ago HOT
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Is this not RTM?  