Group: Forum Members
Posts: 460,
Visits: 5.2K
|
looks like bridging to me especially in those tight rads where the material has scrunched up as you can see its very tight together, the material needs to be pushed into all the corners under vacuum or see if you can get away with using strips of material in those areas and matching the twill direction on the other plies.
|