Hi ya,
I am an Aerospace Engineer working in a project, developing a electric super car and I am manufacturing car body panels using VARI process.
Recently I have came a cross some complecations with the panels that I have manufatured. (Please see the attcahed photos)
As you can see, there is a mist like marks in the corners for this front hood reinforced panel. I used gel coat on the mold.
Does anyone have any idea why I am getting these marks.
and any advise will be appriceated.