Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Hi Finnluxury,
Was this the catch pot or the degassing chamber as only the catch pot comes with a hole in the lid. We would be very interested to know what has caused this as obviously we do not want such equipment failing suddenly in this way! Please do keep us updated on what happened so we can take any action if necessary.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|