By Finnluxury - 6/17/2017 10:04:10 PM
Hi.Last night happened something really weird. I use EC 26L professional vacuum degassing chamber as a resin catch pot (resin trap). So I have 25mm clear acrylic lid, where i have a hole for resin to go inside the chamber. So the weird thing goes like this: I resin infused a carbon fiber front fender just like I normally do. This time only different were that I used IP2 infusion polyester resin instead of Epoxy that i didn't have at the moment. Infusion went very well like usually. I closed the hoses, closed the pump and leaved the part cure over night. When I came back to the warehouse, I saw that the Acrylic lid were missing from the chamber. When I looked more closely there were Acrylic pcs all over the ware house, and 4 bigger parts of the lid. Clearly somekind of explosion have happened during the night. I am usually very carefull to not leave too much resin in the resin trap, that it will not start to gain heat. I even leaved the vacuum to the chamber, so there is no oxygen that the resin could start a fire, and only around 6mm of resin were in the bottom of the chamber. So I am wondering what have happened? I dont believe that the 6mm of polyester have gained heat so much that it would made over pressure and this would happend. Also I dont believe that the vacuum can make the acrylic lid to get broken. I am wondering that maybe the hole middle of the lid for the vacuum hose have something to do with this. Just wanted to share what happened, and maybe someone could have idea what have happened.
|
By oekmont - 6/23/2017 6:07:12 PM
I was wondering why you need such an immense resin trap. Even if I am infusing a whole seven-style hood, wich is basically a third of the whole car, there are only a few drops, if any. I use the ec resin trap more as a safety device for my pump. I have to say that I am always degassing the resin, so there are no airbubbles I need to let through the resin trap. But even if I did, the 400ml seem like plenty of volume for the task. I mean, this are 400g resin for nothing.
|
|