I am currently attempting to make myself a kayak paddle. I have chosen to use a carbon/Kevlar hybrid reinforcement on the front face of the paddle blades, I know that I won't be able to sand that reinforcement any after I infuse it without making a Harry mess of it so I am thinking about spraying a thin coat of epoxy onto the mold before I lay the reinforcements in to sorta after like a clear coat.  
 My question is, Will this effect the strength of the finished part and add much unnecessary weight? 
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
No no, 12-15 'mils', or thou. Meaning 12-15 thousandths of an inch.