By RedLegsGear - 3/15/2017 7:38:41 PM

I am currently attempting to make myself a kayak paddle. I have chosen to use a carbon/Kevlar hybrid reinforcement on the front face of the paddle blades, I know that I won't be able to sand that reinforcement any after I infuse it without making a Harry mess of it so I am thinking about spraying a thin coat of epoxy onto the mold before I lay the reinforcements in to sorta after like a clear coat.  
 My question is, Will this effect the strength of the finished part and add much unnecessary weight? 
By Hanaldo - 4/1/2017 11:11:19 AM

No no, 12-15 'mils', or thou. Meaning 12-15 thousandths of an inch.