Frobisher
Frobisher
Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)
Group: Forum Members
Posts: 14, Visits: 93
Can anyone recommend a tack spray adhesive (preferably available in Australia) for use with Epoxy infusion. 3M Super 77 seems to get mentioned a lot but it sounds like it affectes the surface finish. Cytec Aerofix 3, from what I can determine, is intended for Polyester and Vinyl-ester resins, plus elite composites don't seem to be in business any more to supply it...

Thanks

Dave
Reply
Hanaldo
Hanaldo
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You pretty much summed it up. 

Aerofix 3 is a great product, but it is only compatible with some epoxies (I don't use vinyl for production parts), and unfortunately the infusion epoxy I am using now isn't one of them. 

Also due to the fact that it is DG, and I don't buy any other DG products from Lavender, means that it's quite simply ridiculous to buy. Super 77 gives me the exact same results with epoxy, but I can get it locally for 20 bucks. 