Hi i have just completed the step 11 of the skinning process on my mirror covers. At this stage would it ok to use water with the 120 grit sand paper when flattening he surface for the final coat. 
Also i have got very lunpy rough edges what is the best technique to get them flush right to the edge thank you. 
I will attache pics thank you 
Reply
Shaz
Shaz
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 3, Visits: 7
Cheers warren much appreciated 

Kind regards 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search