Very off topic project I am doing but I am trying to replicate some over quarter fenders for the rear of my 94 rx7, I recently bought the rear over quarters a month ago and they just showed up, anyways these panels are 1100 shipped from japan and I need two sets and I only have one so I have to make a mold to make another set as I have two cars that need them. My question is what materials to use, how to flange this part for a mold, and can I use evercoat pva or do i need wax to release mold from part?
Attachments
IMG_0866.JPG (704 views, 1.00 MB)
IMG_0867.JPG (539 views, 1.00 MB)
IMG_0868.JPG (491 views, 1.00 MB)
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Ok. In that case I would go for 3 layers of 225g and 2 layers of 450g chopped strand. You could use 5 layers of a 260g woven glass too, but woven fabrics are a bit harder to wet-lay without vacuum. 

You could also use a core or bulker mat like Coremat or PVC. In which case I would use a 3mm core with one layer of 225g glass on either side. 