over fender mold need help


Author
Message
bridgeport13b
bridgeport13b
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 17
Very off topic project I am doing but I am trying to replicate some over quarter fenders for the rear of my 94 rx7, I recently bought the rear over quarters a month ago and they just showed up, anyways these panels are 1100 shipped from japan and I need two sets and I only have one so I have to make a mold to make another set as I have two cars that need them. My question is what materials to use, how to flange this part for a mold, and can I use evercoat pva or do i need wax to release mold from part?
Attachments
IMG_0866.JPG (710 views, 1.00 MB)
IMG_0867.JPG (546 views, 1.00 MB)
IMG_0868.JPG (507 views, 1.00 MB)
bridgeport13b
bridgeport13b
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 17
So the part is 4mm thick, so its very thin, should I add in strips of wood and hot glue them in?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
4mm thick is pretty thick for composites! Legal requirement for fibreglass replacement panels is 3mm, so 4mm is absolutely fine. They must be pretty heavy for what they are! 

PVA would be my choice if you can spray it. If you can't spray it then go for wax, but make sure whatever surface coating that's on it is compatible with the tooling gelcoat that you choose to use. PVA will prevent any compatibility issues, wax won't. Test first! 

As for how to flange, have you watched EC's tutorial videos on making a bonnet? Just follow that process and adapt it for your needs. 



bridgeport13b
bridgeport13b
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 17
OK, i did order pva and i am picking up some relase wax pretty soon, what material oz would u use?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
What do you want to make them out of? Carbon fibre, fibreglass, Kevlar? Do you have vacuum equipment or will you be wet-laying these?
bridgeport13b
bridgeport13b
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 17
Hi the parts I am making are going to be fiberglass and I do not have a vacumme source 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Ok. In that case I would go for 3 layers of 225g and 2 layers of 450g chopped strand. You could use 5 layers of a 260g woven glass too, but woven fabrics are a bit harder to wet-lay without vacuum. 

You could also use a core or bulker mat like Coremat or PVC. In which case I would use a 3mm core with one layer of 225g glass on either side. 
joellawtie
joellawtie
Supreme Being (182 reputation)Supreme Being (182 reputation)Supreme Being (182 reputation)Supreme Being (182 reputation)Supreme Being (182 reputation)Supreme Being (182 reputation)Supreme Being (182 reputation)Supreme Being (182 reputation)Supreme Being (182 reputation)
Group: Forum Members
Posts: 20, Visits: 223
I'll be doing the same for my JZZ30 when i get skilled enough with vacuum infusion so im gonna have to follow this and see how you get on dude Smile