Need Help with infusion issue


Author
Message
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
Hello guys started to d infusion , but i dont get why i get this if before starting to allow resin to flow vacuuming gauge showed perfect vacuuming. after i shut down both sides also lok perfect vacuuming but all carbon flat pieces started to go bubbles i dont get where is problem.

https://www.youtube.com/watch?v=jDeB3bKK3mI&feature=youtu.be



Please Master of infusion Wink need your help where i made wrong step?
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
What is the white core you have in there? Looks like coremat?