Need Help with infusion issue
Need Help with infusion issue
Post Reply
Like
3
Need Help with infusion issue
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Hello guys started to d infusion , but i dont get why i get this if before starting to allow resin to flow vacuuming gauge showed perfect vacuuming. after i shut down both sides also lok perfect vacuuming but all carbon flat pieces started to go bubbles i dont get where is problem.
https://www.youtube.com/watch?v=jDeB3bKK3mI&feature=youtu.be
Please Master of infusion
need your help where i made wrong step?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Need Help with infusion issue
TomDesign
-
9 Years Ago
You have a bag leak. The rigid mesh I found a nightmare for perforating the bag. Either get finer,...
ajb100
-
9 Years Ago
where you see leak it holder on number 30 i dont get so how that work
TomDesign
-
9 Years Ago
Your clamp is between the vac bag and catch pot. All that gauge is showing is that your catch pot is...
ajb100
-
9 Years Ago
What is the white core you have in there? Looks like coremat?
Fasta
-
9 Years Ago
ou so to test vacuum is not to turn of those 2 clamps ? as before infusion like that i tested and...
TomDesign
-
9 Years Ago
Also, are you using epoxy or polyester? Hadn't noticed the core when I watched on my phone.
ajb100
-
9 Years Ago
is that has any difference i use epoxy or polyster ? as i dont get why it get leak
TomDesign
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search