By TomDesign - 9/18/2016 4:09:10 PM
Hello guys started to d infusion , but i dont get why i get this if before starting to allow resin to flow vacuuming gauge showed perfect vacuuming. after i shut down both sides also lok perfect vacuuming but all carbon flat pieces started to go bubbles i dont get where is problem.
https://www.youtube.com/watch?v=jDeB3bKK3mI&feature=youtu.be
Please Master of infusion need your help where i made wrong step?
|
By TomDesign - 9/19/2016 11:49:13 AM
is that has any difference i use epoxy or polyster ? as i dont get why it get leak
|
|