Guys

can you imagine i bought seats 1k pounds and it was told no clear coat only polished polyster resin and UV do not affraid bs i think. seats all over the corner air holes.
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Negative, that is one of the benefits of polyester resin. It polishes exceptionally well, and is naturally UV stable. 

As for links, Easy Composites stock them. Their IP2 infusion polyester is an isophthalic resin, and I believe their GP laminating polyester is an orthophthalic. Both are UV stable. 