Tillet carbon seats
Tillet carbon seats
Post Reply
Like
2
Tillet carbon seats
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Guys
can you imagine i bought seats 1k pounds and it was told no clear coat only polished polyster resin and UV do not affraid bs i think. seats all over the corner air holes.
Reply
Like
2
Reply
TomDesign
TomDesign
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
any link on those resins? as i dont think you polish any resin and uv not burn it. all resin not accept uv without clear coat surface to be protected
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Tillet carbon seats
TomDesign
-
9 Years Ago
Well polyester is naturally UV resistant, so if it is laminated with polyester then UV should not...
Hanaldo
-
9 Years Ago
any link on those resins? as i dont think you polish any resin and uv not burn it. all resin not...
TomDesign
-
9 Years Ago
Negative, that is one of the benefits of polyester resin. It polishes exceptionally well, and is...
Hanaldo
-
9 Years Ago
so you want to say people after overlay carbon parts they simply polish parts and dont need to...
TomDesign
-
9 Years Ago
If they are overlaying with polyester and only clear coating for UV protection, then sure. Not...
Hanaldo
-
9 Years Ago
RE: Tillet carbon seats
TomDesign
-
9 Years Ago
RE: Tillet carbon seats
TomDesign
-
9 Years Ago
look all over the seats holes. so you want me to say that when only overlay polyster carbon on top...
TomDesign
-
9 Years Ago
Yeh well, air voids are another matter entirely. And yes, epoxy is not UV stable, it will yellow...
Hanaldo
-
9 Years Ago
ok so i wrap oem piece polish and put on a sun and it wont burn? i dont use epoxy i wrap with...
TomDesign
-
9 Years Ago
It should not yellow or degrade, no.
Hanaldo
-
9 Years Ago
Lets test that ))
TomDesign
-
9 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search