When you say "perfect" what exactly do you want ?
If you want perfect out of the mould your only choice is 2 shot with film glue
You can get some pre preg resin systems that are core bondable (mtm28b for example) that you could do it in one hit with but you will almost certainly need to to lacquer to get a perfect Finnish
A debulk on your 1st ply will help
If you are doing a autoclave cure always use a vented cure
|