Hello!
I am planning to make carbon fiber + nomex honey comb sandwich sheets, about 1.5 m2 pieces. The sheets are not 100% straight, but no radical shapes neither included
The skins would be app 220g/m2 carbon, and inside 4,8mm Nomex, 5mm thick. What are my possibilities?
I red about dipping the honeycomb in epoxy. Also about the adhesive films etc. Even some sources say, that I can do everything in one pass, without glues (when using prepreg).....
Only the surface facing to the mold has to be perfect, other side does not matter at all.
Carbonnewbie