Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Dull mould after release
Dull mould after release
Post Reply
Like
3
Dull mould after release
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
carbon man
carbon man
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 86,
Visits: 1.2K
As title says really. After polishing the mould to hight gloss shine. Then waxing several times ready for the first part to be layed up. I use a polyester gel coat.
The first part come out of the mould ok but my new shiney new mould is now dull?
I don't want to pollish again or I will have to go through the coats of realese wax again.
Any help thanks.
Reply
Like
3
Replies
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Sounds like a small degree of cross linking occurred. This should occur less as you use the mould more. Polish it up again and redo the wax; when using wax you should reapply it with every pull anyway.
Reply
Like
2
carbon man
carbon man
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Awaiting Activation
Posts: 86,
Visits: 1.2K
Where as I apply about 15 coats of wax for first release, do I need do another 15 if I re pollish after the first realese?
Cheers
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Dull mould after release
carbon man
-
9 Years Ago
Sounds like a small degree of cross linking occurred. This should occur less as you use the mould...
Hanaldo
-
9 Years Ago
Where as I apply about 15 coats of wax for first release, do I need do another 15 if I re pollish...
carbon man
-
9 Years Ago
I would do it for the first 3-5 pulls.
Hanaldo
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search