By carbon man - 4/5/2016 1:25:11 PM

As title says really. After polishing the mould to hight gloss shine. Then waxing several times ready for the first part to be layed up. I use a polyester gel coat. 

The first part come out of the mould ok but my new shiney new mould is now dull? 

I don't want to pollish again or I will have to go through the coats of realese wax again. 

Any help thanks. 
By Hanaldo - 4/5/2016 2:25:58 PM

I would do it for the first 3-5 pulls.