HI guys for some reason my pump doesn't seem to be pulling full vaccum, the flow indicator has stopped spinning but the gauge isn't quite at -30
Even with the part clamped off it still doesn't go down to -30 but it did used too what's causing this?  http://www.talkcomposites.com/Uploads/Images/cdb0d1a9-5c6b-429c-a415-f8ce.jpg
Reply
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
Thanks for the replies I thought the tone of the pump had changed but thought I'd ask to make sure 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
111mattin111 - 9 Years Ago
VVS - 9 Years Ago
111mattin111 - 9 Years Ago
Hanaldo - 9 Years Ago
MarkMK - 9 Years Ago
111mattin111 - 9 Years Ago
seense - 9 Years Ago
fgayford - 9 Years Ago
Matt (Staff) - 9 Years Ago
111mattin111 - 9 Years Ago
matthieutje65 - 9 Years Ago
111mattin111 - 9 Years Ago
Hanaldo - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search