Hello guys and girls

Has anyone had any practical experience thinning epoxy resin for infusion ?

I have been advised that if I use MEK at no more than 2% in the part A  it will be ok.

I understand that there may be a reduction in strength which wont be an issue for the parts I make.



Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
never done that but heard about that as well...
Can I ask you why you just don't buy resin for infusion and save you all the trouble and stress of everything working out well? Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search