http://www.ebay.com.au/itm/201425740216?_trksid=p2057872.m2749.l2649&ssPageName=STRK%3AMEBIDX%3AIT




Had a real hard time removing flow media and peel ply from a fairly complex mould. Do you think this perforated release film would be ok between the flow media and the peel ply ?

perforations are 0.8mm or  .031"   at 5mm spacing




Thanks




Rod.









Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh I can see why it would make removing the consumables hard. 

I think you're making life harder than it needs to be though, there's no need to feed the tube through the mould? Just infuse it regularly with a infusion connector. 
rallyfly
rallyfly
Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)
Group: Forum Members
Posts: 25, Visits: 85
Your probably right bud , I just thought I could get a more reliable seal on a nice flat surface rather than wrinkly vac bag.  I have sanded the aft sides nice and smooth and flat where the tubes go through.

I use  flanged bush which slides over the tube and sealed with a tack tape doughnut against the mould.