Breather layer cloth?


Author
Message
67redrocket
67redrocket
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 49, Visits: 486
I bought a infusion starter kit from EC. In this kit I got a couple square meters of breather layer cloth. I have seen the instructions film on easy composites.com, but I have't seen a film with the breather cloth in use. So I have some questions:

- When should I use the breather cloth?
- Why do I use the breather cloth? 
- How do I use the breather cloth?
Reply
Grace James
Grace James
Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)
Group: Forum Members
Posts: 2, Visits: 32
Cameron Bartlett - 7/19/2021 5:29:09 PM
Is breather cloth necessary for a large (1500mm x 500mmx30mm), wet layup? I'm making a centerboard for my sailboat and i'm trying to figure out if i can DIY a vacuum setup with my home or shop vacuum.  I'm wondering if it is necessary to use breather fabric? I don't care about looks, only strength.  Thanks

Well...since you want to do wet layup, I think that breather cloth isn't necessary. Remember to use peel ply and a net. 

Good luck.