Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Breather layer cloth?
Breather layer cloth?
Post Reply
Like
4
Breather layer cloth?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
67redrocket
67redrocket
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I bought a infusion starter kit from EC. In this kit I got a couple square meters of breather layer cloth. I have seen the instructions film on easy composites.com, but I have't seen a film with the breather cloth in use. So I have some questions:
- When should I use the breather cloth?
- Why do I use the breather cloth?
- How do I use the breather cloth?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Breather layer cloth?
67redrocket
-
11 Years Ago
Assuming it's the white cloth akin to a thin blanket, then you shouldn't need it for infusion, not...
MarkMK
-
11 Years Ago
Hi RedRocket; the Breather Fabric is something which we constantly consider as to whether it should...
Rich (Staff)
-
11 Years Ago
Is breather cloth necessary for a large (1500mm x 500mmx30mm), wet layup? I'm making a centerboard for my sailboat and i'm trying to figure out if i can DIY a vacuum setup with my home or shop vacuum...
Cameron Bartlett
-
5 Years Ago
Well...since you want to do wet layup, I think that breather cloth isn't necessary. Remember to use peel ply and a net. Good luck.
Xaris James
-
5 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search