67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
Have anyone used this spray tack on carbon fiber and epoxy infusion? How was the result?
Reply
Like
3
Reply
carbonfibreworks
carbonfibreworks
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Hi Redrocket
I have not used the product mentioned but have tried most others and you really need to avoid a spray adhesive on the first layer of carbon if you are making a cosmetic part or having the carbon visible as they all impact on the finish of the component to some extent.
Chris
Carbon fibre works LTD
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
NautiGrip IF spray adhesive
67redrocket
-
10 Years Ago
Hi Redrocket I have not used the product mentioned but have tried most others and you really need to...
carbonfibreworks
-
10 Years Ago
Should diluted epoxy resin from a spray bottle also be avoided on cosmetic parts? How do I then...
67redrocket
-
10 Years Ago
Hi Redrocket It helps with complex shapes to use a woven infusion mesh and pull the bag down slowly...
carbonfibreworks
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search