NautiGrip IF spray adhesive

http://www.talkcomposites.com/Topic19406.aspx

By 67redrocket - 10/1/2015 1:57:46 PM

Have anyone used this spray tack on carbon fiber and epoxy infusion? How was the result?
By carbonfibreworks - 10/1/2015 6:08:03 PM

Hi Redrocket
It helps with complex shapes to use a woven infusion mesh and pull the bag down slowly and push the carbon and stack into place, you can use rounded plastic tools but be careful as you may damage the bag. You can also make and use use silicone intensifiers.
Regards Chris
Carbon fibre works LTD