Carbon fibre/ glass fibre laminate/ Glass fibre "skinning"


Author
Message
maggie
maggie
Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)
Group: Forum Members
Posts: 7, Visits: 43
Hi,

      I am interested in thoughts as to reasons for using a glass fibre (Such as woven glass 2/2 twill) layer with woven carbon fibre layer in a laminate.

My thoughts are corrosion resistance of a metal part if next to the glass and cost.

What difficulties are presented ?

Any illustrations of examples.

Could twill weave glass fibre be used for skinning.   Smile






Dravis
Dravis
Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Yes .. Glass fibre twill can be used for "skinning"  --- in a single layer it will be nearly transparent though .. it will not hide the material underneath Cool

I have successfully "skinned" wood parts with light weight woven glassfibre, and you can not really tell that the glass is there, it just looks like a very thick varnish.

Glass fibre is non conductive, and as such one choice for a "corrosion protective layer" between CF and metal parts.  Other choices are Diolene and pure Kevlars.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Warren (Staff)
Warren (Staff)
Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
From a structural perspective, glass fibre is fine for skinning but not as high a performance material as carbon fibre.

Corrosion between conductive metals can be prevented with a thin layer of glass fibre or resin between the two metals.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search